| PTN101 | 显著提升:镁铝合金、镀锌板、不锈钢、电泳漆上粉末涂层的附着力,包括涂层间的附着力 Significantly improve: Adhesion of powder coatings on magnesium-aluminum alloy, galvanized sheet, stainless steel, and electrophoretic paint, including inter-coat adhesion | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN102 | 显著提升:铝合金、钢铁基材上的附着力,解决因为油污和锈点导致的附着力下降问题 Significantly improve: Adhesion on aluminum alloy and steel substrates, solve the problem of decreased adhesion caused by oil stains and rust spots | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN103 | 改善铸铁、铸铝、不锈钢、锌合金上粉末涂层的附着力,有效改善涂层与底材的粘结力和柔韧性 Improve the adhesion of powder coatings on cast iron, cast aluminum, stainless steel, and zinc alloy, effectively improve the bonding strength and flexibility between the coating and the substrate | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN104 | 改善镁合金、镀锌板、不锈钢、铸铁、铸铝等底材上粉末涂层的附着力,加强延迟附着力 Improve the adhesion of powder coatings on substrates such as magnesium alloy, galvanized sheet, stainless steel, cast iron, and cast aluminum, strengthen delayed adhesion | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN105 | 显著提升:PVC、ABS等非金属材料上粉末涂层的附着力,包括层间附着力 Significantly improve: Adhesion of powder coatings on non-metallic materials such as PVC and ABS, including interlayer adhesion | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN106 | 显著提升:高温粉末涂层对金属底材的附着力和耐久性,改善高温烘烤产生的粉化和脱落现象 Significantly improve: Adhesion and durability of high-temperature powder coatings to metal substrates, improve powdering and peeling phenomena caused by high-temperature baking | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN107 | 应用于纯环氧防腐和绝缘粉末涂料,不仅可以提升附着力,同时提升耐水性、耐盐雾和耐阴极剥离等性能 Applied to pure epoxy anti-corrosion and insulating powder coatings, it can not only improve adhesion, but also improve water resistance, salt spray resistance, and cathodic disbondment resistance | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |
| PTN108 | 有效提升各种冷镀锌、热镀锌基材上的附着力 Effectively improve adhesion on various cold galvanized and hot-dip galvanized substrates | 0.5-1.5%(预混) 0.5-1.5% (pre-blending) |